PropertyDIN Ck60DIN RSt37-2Difference
Yield strength400 MPa225 MPa-44%
Tensile strength680 MPa340 MPa-50%
Elongation13 %26 %+100%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K66.5 W/m·K+28%
Specific heat467 J/kg·K456 J/kg·K-2%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN RSt37-2 relative to DIN Ck60. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck60
standard
DIN
heat treatment
normalized
DIN RSt37-2
standard
DIN
heat treatment

What else is in Engineering Database

Related comparisons

View each material