Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
DIN 28Mn6 vs DIN 30CrNiMo8
Property comparison of DIN 28Mn6 and DIN 30CrNiMo8, both carbon steel.
| Property | DIN 28Mn6 | DIN 30CrNiMo8 | Difference |
|---|---|---|---|
| Yield strength | 490 MPa | 1,050 MPa | +114% |
| Tensile strength | 690 MPa | 1,250 MPa | +81% |
| Elongation | 15 % | 9 % | -40% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 62.4 W/m·K | 61.6 W/m·K | -1% |
| Specific heat | 459 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is DIN 30CrNiMo8 relative to DIN 28Mn6. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
DIN 28Mn6
- standard
- DIN
DIN 30CrNiMo8
- standard
- DIN
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators