Home/Compare/Carbon Steel/DIN 17CrNiMo6 vs DIN 17Mn4

DIN 17CrNiMo6 vs DIN 17Mn4

Property comparison of DIN 17CrNiMo6 and DIN 17Mn4, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN 17CrNiMo6DIN 17Mn4Difference
Yield strength785 MPa290 MPa-63%
Tensile strength1,080 MPa460 MPa-57%
Elongation8 %22 %+175%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.5 W/m·K66.5 W/m·K0%
Specific heat456 J/kg·K456 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN 17Mn4 relative to DIN 17CrNiMo6. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.