Property comparison of DIN 17Cr3 and DIN 25CrMo4, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN 17Cr3DIN 25CrMo4Difference
Yield strength340 MPa600 MPa+76%
Tensile strength590 MPa800 MPa+36%
Elongation13 %14 %+8%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.5 W/m·K63.5 W/m·K-5%
Specific heat456 J/kg·K458 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN 25CrMo4 relative to DIN 17Cr3. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.