Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/DIN 10Ni14 vs DIN 13CrMo4

DIN 10Ni14 vs DIN 13CrMo4

Property comparison of DIN 10Ni14 and DIN 13CrMo4, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN 10Ni14DIN 13CrMo4Difference
Yield strength355 MPa295 MPa-17%
Tensile strength490 MPa450 MPa-8%
Elongation22 %20 %-9%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity69.2 W/m·K68.1 W/m·K-2%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN 13CrMo4 relative to DIN 10Ni14. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN 10Ni14
standard
DIN
DIN 13CrMo4
standard
DIN

What else is in Engineering Database

Related comparisons