Stainless Steel4 compared properties
PropertyCustom 465 Stainless Steel Bar H950SAE 409 Stainless Steel (Annealed bar)Difference
Yield strength1,517 MPa240 MPa-84%
Tensile strength1,655 MPa450 MPa-73%
Shear modulus197,880 MPa74,231 MPa-62%
Coefficient of thermal expansion0 1/K0.000011 1/K+6648%

Difference is SAE 409 Stainless Steel (Annealed bar) relative to Custom 465 Stainless Steel Bar H950. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Custom 465 Stainless Steel Bar H950
grade
Custom 465
standard
MIL-HDBK-5J
heat treatment
H950
SAE 409 Stainless Steel (Annealed bar)
grade
409
standard
SAE
heat treatment
Annealed bar

About 400-series stainless steels

Martensitic and ferritic stainless steels carry less nickel than the 300-series and remain magnetic. 410 and 420 are hardenable by quench and temper and are used for cutlery, shafts, and valve parts. 430 stays soft and is used for cosmetic trim and mild corrosion service. Compared to 300-series grades they trade general corrosion resistance for hardenability.

What else is in Engineering Database

Related comparisons

View each material