CSN 423256 vs CSN 423311

Property comparison of CSN 423256 and CSN 423311, both copper alloy.

Copper Alloy10 compared properties
PropertyCSN 423256CSN 423311Difference
Yield strength255 MPa350 MPa+37%
Tensile strength350 MPa600 MPa+71%
Elastic modulus100,000 MPa100,000 MPa0%
Shear modulus37,000 MPa37,000 MPa0%
Poisson ratio0.340.340%
Density8,700 kg/m³8,700 kg/m³0%
Thermal conductivity75 W/m·K75 W/m·K0%
Specific heat385 J/kg·K385 J/kg·K0%
Coefficient of thermal expansion0.000018 1/K0.000018 1/K0%
Melting point960 °C960 °C0%

Difference is CSN 423311 relative to CSN 423256. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.