CSN 423047 vs CSN 423123

Property comparison of CSN 423047 and CSN 423123, both copper alloy.

Copper Alloy10 compared properties
PropertyCSN 423047CSN 423123Difference
Yield strength265 MPa160 MPa-40%
Tensile strength380 MPa180 MPa-53%
Elastic modulus120,000 MPa105,000 MPa-13%
Shear modulus45,000 MPa40,000 MPa-11%
Poisson ratio0.310.310%
Density8,700 kg/m³8,700 kg/m³0%
Thermal conductivity75 W/m·K75 W/m·K0%
Specific heat385 J/kg·K385 J/kg·K0%
Coefficient of thermal expansion0.000018 1/K0.000018 1/K0%
Melting point960 °C960 °C0%

Difference is CSN 423123 relative to CSN 423047. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.