Home/Compare/Cast Iron/CSN 422305 vs CSN 422307

CSN 422305 vs CSN 422307

Property comparison of CSN 422305 and CSN 422307, both cast iron.

Cast Iron10 compared properties
PropertyCSN 422305CSN 422307Difference
Yield strength320 MPa420 MPa+31%
Tensile strength500 MPa700 MPa+40%
Elastic modulus169,000 MPa169,000 MPa0%
Shear modulus70,000 MPa70,000 MPa0%
Poisson ratio0.20.20%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422307 relative to CSN 422305. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.