Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/CSN 16640 vs CSN 17021

CSN 16640 vs CSN 17021

Property comparison of CSN 16640 and CSN 17021, both carbon steel.

Carbon Steel10 compared properties
PropertyCSN 16640CSN 17021Difference
Yield strength1,275 MPa415 MPa-67%
Tensile strength1,569 MPa590 MPa-62%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat462 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is CSN 17021 relative to CSN 16640. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

CSN 16640
standard
CSN
heat treatment
heat treated
CSN 17021
standard
CSN
heat treatment
normalized