Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/CSN 16343 vs CSN 16420

CSN 16343 vs CSN 16420

Property comparison of CSN 16343 and CSN 16420, both carbon steel.

Carbon Steel11 compared properties
PropertyCSN 16343CSN 16420Difference
Yield strength900 MPa785 MPa-13%
Tensile strength1,100 MPa932 MPa-15%
Elongation10 %10 %0%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat463 J/kg·K457 J/kg·K-1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is CSN 16420 relative to CSN 16343. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

CSN 16343
standard
CSN
heat treatment
CSN 16420
standard
CSN
heat treatment
case-hardened

What else is in Engineering Database

Related comparisons

View each material