CSN 12071 vs CSN 13030
Property comparison of CSN 12071 and CSN 13030, both carbon steel.
| Property | CSN 12071 | CSN 13030 | Difference |
|---|---|---|---|
| Yield strength | 1,470 MPa | 285 MPa | -81% |
| Tensile strength | 1,770 MPa | 460 MPa | -74% |
| Elongation | 2 % | 21 % | +950% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 49.4 W/m·K | 51.9 W/m·K | +5% |
| Specific heat | 468 J/kg·K | 460 J/kg·K | -2% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is CSN 13030 relative to CSN 12071. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
CSN 12071
- standard
- CSN
- heat treatment
- heat treated
CSN 13030
- standard
- CSN
- heat treatment
- —
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators