PropertyCopper-Nickel C96200Copper-Nickel C96400Difference
Yield strength172 MPa255 MPa+48%
Tensile strength310 MPa469 MPa+51%
Elongation20 %28 %+40%
Elastic modulus100,000 MPa100,000 MPa0%
Shear modulus37,000 MPa37,000 MPa0%
Poisson ratio0.340.340%
Density8,940 kg/m³8,940 kg/m³0%
Thermal conductivity25 W/m·K25 W/m·K0%
Specific heat394 J/kg·K394 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,100 °C1,100 °C0%

Difference is Copper-Nickel C96400 relative to Copper-Nickel C96200. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Copper-Nickel C96200
standard
ANSI
Copper-Nickel C96400
standard
ANSI

What else is in Engineering Database

Related comparisons

View each material