Copper Alloy11 compared properties
PropertyCopper Alloy C75200Copper Alloy C75700Difference
Yield strength172 MPa124 MPa-28%
Tensile strength386 MPa359 MPa-7%
Elongation45 %48 %+7%
Elastic modulus105,000 MPa105,000 MPa0%
Shear modulus40,000 MPa40,000 MPa0%
Poisson ratio0.320.320%
Density8,730 kg/m³8,730 kg/m³0%
Thermal conductivity27 W/m·K27 W/m·K0%
Specific heat394 J/kg·K394 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,010 °C1,010 °C0%

Difference is Copper Alloy C75700 relative to Copper Alloy C75200. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Copper Alloy C75200
standard
ANSI
Copper Alloy C75700
standard
ANSI

What else is in Engineering Database

Related comparisons

View each material