Copper Alloy C69000 vs Copper Alloy C69400
Property comparison of Copper Alloy C69000 and Copper Alloy C69400, both copper alloy.
| Property | Copper Alloy C69000 | Copper Alloy C69400 | Difference |
|---|---|---|---|
| Yield strength | 359 MPa | 276 MPa | -23% |
| Tensile strength | 565 MPa | 552 MPa | -2% |
| Elongation | 35 % | 25 % | -29% |
| Elastic modulus | 105,000 MPa | 105,000 MPa | 0% |
| Shear modulus | 40,000 MPa | 40,000 MPa | 0% |
| Poisson ratio | 0.32 | 0.32 | 0% |
| Density | 8,360 kg/m³ | 8,360 kg/m³ | 0% |
| Thermal conductivity | 87 W/m·K | 87 W/m·K | 0% |
| Specific heat | 385 J/kg·K | 385 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000018 1/K | 0.000018 1/K | 0% |
| Melting point | 900 °C | 900 °C | 0% |
Difference is Copper Alloy C69400 relative to Copper Alloy C69000. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- ANSI
- standard
- ANSI
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators