Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Copper Alloy/Copper Alloy C65100 vs Copper Alloy C65500

Copper Alloy C65100 vs Copper Alloy C65500

Property comparison of Copper Alloy C65100 and Copper Alloy C65500, both copper alloy.

Copper Alloy11 compared properties
PropertyCopper Alloy C65100Copper Alloy C65500Difference
Yield strength103 MPa145 MPa+41%
Tensile strength276 MPa386 MPa+40%
Elongation55 %63 %+15%
Elastic modulus105,000 MPa105,000 MPa0%
Shear modulus40,000 MPa40,000 MPa0%
Poisson ratio0.320.320%
Density8,530 kg/m³8,530 kg/m³0%
Thermal conductivity55 W/m·K55 W/m·K0%
Specific heat380 J/kg·K380 J/kg·K0%
Coefficient of thermal expansion0.000018 1/K0.000018 1/K0%
Melting point970 °C970 °C0%

Difference is Copper Alloy C65500 relative to Copper Alloy C65100. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.