Copper Alloy11 compared properties
PropertyCopper Alloy C61400Copper Alloy C61800Difference
Yield strength228 MPa269 MPa+18%
Tensile strength524 MPa552 MPa+5%
Elongation45 %28 %-38%
Elastic modulus105,000 MPa105,000 MPa0%
Shear modulus40,000 MPa40,000 MPa0%
Poisson ratio0.320.320%
Density7,780 kg/m³7,780 kg/m³0%
Thermal conductivity56 W/m·K56 W/m·K0%
Specific heat410 J/kg·K410 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,040 °C1,040 °C0%

Difference is Copper Alloy C61800 relative to Copper Alloy C61400. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Copper Alloy C61400
standard
ANSI
Copper Alloy C61800
standard
ANSI

What else is in Engineering Database

Related comparisons

View each material