Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Lead Alloy/Chemical Lead (Pb-0.04–0.08Cu) vs Pure Lead (Pb 99.94% min)

Chemical Lead (Pb-0.04–0.08Cu) vs Pure Lead (Pb 99.94% min)

Property comparison of Chemical Lead (Pb-0.04–0.08Cu) and Pure Lead (Pb 99.94% min), both lead alloy.

Lead Alloy10 compared properties
PropertyChemical Lead (Pb-0.04–0.08Cu)Pure Lead (Pb 99.94% min)Difference
Yield strength8 MPa6 MPa-25%
Tensile strength20 MPa18 MPa-10%
Elongation45 %50 %+11%
Elastic modulus16,000 MPa16,000 MPa0%
Density11,340 kg/m³11,340 kg/m³0%
Brinell hardness5 HB4 HB-20%
Thermal conductivity35 W/m·K35 W/m·K0%
Specific heat128 J/kg·K128 J/kg·K0%
Coefficient of thermal expansion0.000029 1/K0.000029 1/K0%
Melting point327 °C327 °C0%

Difference is Pure Lead (Pb 99.94% min) relative to Chemical Lead (Pb-0.04–0.08Cu). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Chemical Lead (Pb-0.04–0.08Cu)
grade
copper-bearing lead
standard
ASTM B29
heat treatment
as-cast/wrought
Pure Lead (Pb 99.94% min)
grade
refined pure lead
standard
ASTM B29
heat treatment
as-cast/wrought