Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Graphite/Carbon Fiber PAN-based (IM7 intermediate modulus) vs Carbon Fiber Pitch-based High Modulus (K1100 / Thornel)

Carbon Fiber PAN-based (IM7 intermediate modulus) vs Carbon Fiber Pitch-based High Modulus (K1100 / Thornel)

Property comparison of Carbon Fiber PAN-based (IM7 intermediate modulus) and Carbon Fiber Pitch-based High Modulus (K1100 / Thornel), both carbon graphite.

Carbon Graphite6 compared properties
PropertyCarbon Fiber PAN-based (IM7 intermediate modulus)Carbon Fiber Pitch-based High Modulus (K1100 / Thornel)Difference
Tensile strength5,516 MPa2,410 MPa-56%
Elongation1.9 %0.25 %-87%
Density1,780 kg/m³2,130 kg/m³+20%
Thermal conductivity4 W/m·K600 W/m·K+14900%
Specific heat710 J/kg·K710 J/kg·K0%
Coefficient of thermal expansion-0 1/K-0.000002 1/K-300%

Difference is Carbon Fiber Pitch-based High Modulus (K1100 / Thornel) relative to Carbon Fiber PAN-based (IM7 intermediate modulus). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

What else is in Engineering Database

Related comparisons

View each material