PropertyBS 55EBS 708M40Difference
Yield strength430 MPa740 MPa+72%
Tensile strength550 MPa925 MPa+68%
Elongation19 %12 %-37%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity65.4 W/m·K51.9 W/m·K-21%
Specific heat457 J/kg·K462 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is BS 708M40 relative to BS 55E. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

BS 55E
standard
BS
heat treatment
BS 708M40
standard
BS
heat treatment
face hardened

What else is in Engineering Database

Related comparisons

View each material