Black Cherry clear dry wood vs Douglas Fir (coast) clear dry wood
Property comparison of Black Cherry clear dry wood and Douglas Fir (coast) clear dry wood, both wood.
| Property | Black Cherry clear dry wood | Douglas Fir (coast) clear dry wood | Difference |
|---|---|---|---|
| Elastic modulus | 10,300 MPa | 13,800 MPa | +34% |
| Poisson ratio | 0.392 | 0.29 | -26% |
| Density | 500 kg/m³ | 490 kg/m³ | -2% |
| Thermal conductivity | 0.15 W/m·K | 0.12 W/m·K | -20% |
Difference is Douglas Fir (coast) clear dry wood relative to Black Cherry clear dry wood. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- USDA FPL-GTR-190
- standard
- USDA
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators