Wood7 compared properties
PropertyBalsa (Ochroma pyramidale) clear dry woodHard Maple (Sugar Maple) clear dry woodDifference
Tensile strength3 MPa65 MPa+2067%
Elastic modulus3,400 MPa12,600 MPa+271%
Poisson ratio0.230.3+30%
Density170 kg/m³740 kg/m³+335%
Thermal conductivity0.055 W/m·K0.18 W/m·K+227%
Specific heat1,640 J/kg·K1,640 J/kg·K0%
Coefficient of thermal expansion0.000005 1/K0.000006 1/K+12%

Difference is Hard Maple (Sugar Maple) clear dry wood relative to Balsa (Ochroma pyramidale) clear dry wood. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Balsa (Ochroma pyramidale) clear dry wood
standard
USDA
Hard Maple (Sugar Maple) clear dry wood
standard
USDA