Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI S240 (Martensitic PH) vs Ph15 7MO

ATI S240 (Martensitic PH) vs Ph15 7MO

Property comparison of ATI S240 (Martensitic PH) and Ph15 7MO, both stainless steel.

Stainless Steel4 compared properties
PropertyATI S240 (Martensitic PH)Ph15 7MODifference
Yield strength1,600 MPa1,138 MPa-29%
Tensile strength1,689 MPa1,276 MPa-24%
Elastic modulus179,300 MPa199,948 MPa+12%
Density7,770 kg/m³7,667 kg/m³-1%

Difference is Ph15 7MO relative to ATI S240 (Martensitic PH). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI S240 (Martensitic PH)
grade
UNS S11900
standard
AMS 5929
heat treatment
Solution Annealed + Aged H950 (510°C)
Ph15 7MO
grade
PH15-7Mo
standard
MIL-HDBK-5J
heat treatment
TH1050

About precipitation-hardening stainless steels

PH grades reach high strength through aging at intermediate temperatures while keeping the corrosion resistance of austenitic or martensitic grades. 17-4 PH and 15-5 PH are the common bar and forging stocks for aerospace and pump shafts. Mechanical properties depend strongly on the aging condition (H900, H1025, H1150).

What else is in Engineering Database

Related comparisons

View each material