Home/Compare/Stainless Steel/ATI 439HP Ferritic Stainless Steel vs ATI 441HP Ferritic Stainless Steel

ATI 439HP Ferritic Stainless Steel vs ATI 441HP Ferritic Stainless Steel

Property comparison of ATI 439HP Ferritic Stainless Steel and ATI 441HP Ferritic Stainless Steel, both stainless steel.

Stainless Steel6 compared properties
PropertyATI 439HP Ferritic Stainless SteelATI 441HP Ferritic Stainless SteelDifference
Yield strength290 MPa310 MPa+7%
Tensile strength455 MPa496 MPa+9%
Elongation34 %31 %-9%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,695 kg/m³7,711 kg/m³0%
Coefficient of thermal expansion0.00001 1/K0.00001 1/K0%

Difference is ATI 441HP Ferritic Stainless Steel relative to ATI 439HP Ferritic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 439HP Ferritic Stainless Steel
grade
UNS S43035
standard
ASTM A240/A268/A479
heat treatment
Annealed
ATI 441HP Ferritic Stainless Steel
grade
UNS S44100
standard
ASTM A240/A554
heat treatment
Annealed

About ferritic stainless steels

Ferritic stainless steels are magnetic, body-centered cubic, and cannot be hardened by heat treatment. They are cheaper than austenitic grades because they carry little or no nickel. 409 and 439 are the standard automotive exhaust grades; 444 and the superferritic grades (29-4C, E-Brite) handle chloride and seawater service better than 316 at lower nickel cost.