Home/Compare/Stainless Steel/ATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust) vs ATI 610 (High-Si Austenitic)

ATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust) vs ATI 610 (High-Si Austenitic)

Property comparison of ATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust) and ATI 610 (High-Si Austenitic), both stainless steel.

Stainless Steel5 compared properties
PropertyATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust)ATI 610 (High-Si Austenitic)Difference
Yield strength260 MPa323 MPa+24%
Tensile strength565 MPa710 MPa+26%
Elongation50 %58 %+16%
Elastic modulus200,000 MPa193,000 MPa-4%
Density7,930 kg/m³7,674 kg/m³-3%

Difference is ATI 610 (High-Si Austenitic) relative to ATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 334Mo Austenitic Stainless Steel (Lean Ni, Automotive Exhaust)
grade
334Mo
standard
ASTM A240
heat treatment
Annealed
ATI 610 (High-Si Austenitic)
grade
UNS S30600
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.