Stainless Steel5 compared properties
PropertyATI 304L Austenitic Stainless Steel (Low Carbon)ATI 31 (Superaustenitic)Difference
Yield strength170 MPa276 MPa+62%
Tensile strength485 MPa650 MPa+34%
Elongation40 %40 %0%
Elastic modulus200,000 MPa198,000 MPa-1%
Density7,900 kg/m³8,060 kg/m³+2%

Difference is ATI 31 (Superaustenitic) relative to ATI 304L Austenitic Stainless Steel (Low Carbon). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 304L Austenitic Stainless Steel (Low Carbon)
grade
304L
standard
ASTM A240
heat treatment
Annealed
ATI 31 (Superaustenitic)
grade
UNS N08031
standard
ASTM B625; EN 1.4562
heat treatment
Solution Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material