| Property | ATI 2102 (Lean Duplex) | ATI 255 (Super Duplex) | Difference |
|---|---|---|---|
| Yield strength | 450 MPa | 551 MPa | +22% |
| Tensile strength | 655 MPa | 758 MPa | +16% |
| Elongation | 30 % | 15 % | -50% |
| Elastic modulus | 200,000 MPa | 200,000 MPa | 0% |
| Density | 7,750 kg/m³ | 7,728 kg/m³ | 0% |
| Brinell hardness | 293 HB | 302 HB | +3% |
| Thermal conductivity | 15.7 W/m·K | 13.3 W/m·K | -15% |
| Coefficient of thermal expansion | 0.000013 1/K | 0.000012 1/K | -8% |
Difference is ATI 255 (Super Duplex) relative to ATI 2102 (Lean Duplex). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- UNS S82011
- standard
- ASTM A240
- heat treatment
- Annealed
- grade
- UNS S32550
- standard
- ASTM A240
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators