ASTM A706 Grade 60 Low-Alloy Seismic Rebar vs ASTM A706 Grade 80 Low-Alloy Seismic Rebar
Property comparison of ASTM A706 Grade 60 Low-Alloy Seismic Rebar and ASTM A706 Grade 80 Low-Alloy Seismic Rebar, both carbon steel.
| Property | ASTM A706 Grade 60 Low-Alloy Seismic Rebar | ASTM A706 Grade 80 Low-Alloy Seismic Rebar | Difference |
|---|---|---|---|
| Yield strength | 414 MPa | 552 MPa | +33% |
| Tensile strength | 552 MPa | 690 MPa | +25% |
| Elongation | 12 % | 12 % | 0% |
| Elastic modulus | 200,000 MPa | 200,000 MPa | 0% |
| Shear modulus | 76,923 MPa | 76,923 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,850 kg/m³ | 7,850 kg/m³ | 0% |
| Thermal conductivity | 61.6 W/m·K | 61.6 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is ASTM A706 Grade 80 Low-Alloy Seismic Rebar relative to ASTM A706 Grade 60 Low-Alloy Seismic Rebar. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- 60
- standard
- ASTM
- grade
- 80
- standard
- ASTM
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators