Aluminum Bronze C95800 vs Commercial bronze C22000
Property comparison of Aluminum Bronze C95800 and Commercial bronze C22000, both aluminum alloy.
| Property | Aluminum Bronze C95800 | Commercial bronze C22000 | Difference |
|---|---|---|---|
| Yield strength | 262 MPa | 69 MPa | -74% |
| Tensile strength | 655 MPa | 255 MPa | -61% |
| Elongation | 25 % | 50 % | +100% |
| Elastic modulus | 120,000 MPa | 105,000 MPa | -13% |
| Shear modulus | 45,000 MPa | 40,000 MPa | -11% |
| Poisson ratio | 0.32 | 0.32 | 0% |
| Density | 8,800 kg/m³ | 8,800 kg/m³ | 0% |
| Thermal conductivity | 155 W/m·K | 155 W/m·K | 0% |
| Specific heat | 900 J/kg·K | 900 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000023 1/K | 0.000023 1/K | 0% |
| Melting point | 580 °C | 580 °C | 0% |
Difference is Commercial bronze C22000 relative to Aluminum Bronze C95800. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- ANSI
- standard
- ANSI
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators