Property comparison of Aluminum Alloy Alclad 7178-O and Aluminum Alloy Alclad 7178-T651, both aluminum alloy.

Aluminum Alloy11 compared properties
PropertyAluminum Alloy Alclad 7178-OAluminum Alloy Alclad 7178-T651Difference
Yield strength97 MPa490 MPa+405%
Tensile strength221 MPa558 MPa+152%
Elongation16 %10 %-38%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Thermal conductivity130 W/m·K130 W/m·K0%
Specific heat856 J/kg·K856 J/kg·K0%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point477 °C477 °C0%

Difference is Aluminum Alloy Alclad 7178-T651 relative to Aluminum Alloy Alclad 7178-O. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy Alclad 7178-O
standard
ANSI
heat treatment
Wrought
Aluminum Alloy Alclad 7178-T651
standard
ANSI
heat treatment
Wrought

About 7xxx aluminum alloys