Aluminum Alloy 5457-H38 vs Aluminum Alloy 5652-H32

Property comparison of Aluminum Alloy 5457-H38 and Aluminum Alloy 5652-H32, both aluminum alloy.

Aluminum Alloy12 compared properties
PropertyAluminum Alloy 5457-H38Aluminum Alloy 5652-H32Difference
Yield strength186 MPa193 MPa+4%
Tensile strength207 MPa228 MPa+10%
Elongation6 %12 %+100%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness55 HB60 HB+9%
Thermal conductivity117 W/m·K117 W/m·K0%
Specific heat900 J/kg·K880 J/kg·K-2%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point568 °C568 °C0%

Difference is Aluminum Alloy 5652-H32 relative to Aluminum Alloy 5457-H38. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 5457-H38
standard
ANSI
heat treatment
Wrought
Aluminum Alloy 5652-H32
standard
ANSI
heat treatment
Wrought

About 5xxx aluminum alloys

5xxx aluminum alloys are alloyed with magnesium. They are not heat-treatable and gain strength through cold work. They have the best corrosion resistance of the wrought aluminums in marine environments. 5052 covers general sheet work; 5083 and 5086 are common in shipbuilding and pressure vessels.