Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/Aluminum Alloy 5254-H112 vs Aluminum Alloy 5254-H34

Aluminum Alloy 5254-H112 vs Aluminum Alloy 5254-H34

Property comparison of Aluminum Alloy 5254-H112 and Aluminum Alloy 5254-H34, both aluminum alloy.

Aluminum Alloy12 compared properties
PropertyAluminum Alloy 5254-H112Aluminum Alloy 5254-H34Difference
Yield strength117 MPa228 MPa+95%
Tensile strength241 MPa290 MPa+20%
Elongation25 %13 %-48%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness63 HB73 HB+16%
Thermal conductivity117 W/m·K117 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point568 °C568 °C0%

Difference is Aluminum Alloy 5254-H34 relative to Aluminum Alloy 5254-H112. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 5254-H112
standard
ANSI
heat treatment
Wrought
Aluminum Alloy 5254-H34
standard
ANSI
heat treatment
Wrought

About 5xxx aluminum alloys

5xxx aluminum alloys are alloyed with magnesium. They are not heat-treatable and gain strength through cold work. They have the best corrosion resistance of the wrought aluminums in marine environments. 5052 covers general sheet work; 5083 and 5086 are common in shipbuilding and pressure vessels.

What else is in Engineering Database

Related comparisons

View each material