Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/Aluminum Alloy 5252-H38 vs Aluminum Alloy 5254-H32

Aluminum Alloy 5252-H38 vs Aluminum Alloy 5254-H32

Property comparison of Aluminum Alloy 5252-H38 and Aluminum Alloy 5254-H32, both aluminum alloy.

Aluminum Alloy12 compared properties
PropertyAluminum Alloy 5252-H38Aluminum Alloy 5254-H32Difference
Yield strength241 MPa207 MPa-14%
Tensile strength283 MPa269 MPa-5%
Elongation5 %15 %+200%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness75 HB67 HB-11%
Thermal conductivity117 W/m·K117 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point568 °C568 °C0%

Difference is Aluminum Alloy 5254-H32 relative to Aluminum Alloy 5252-H38. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 5252-H38
standard
ANSI
heat treatment
Wrought
Aluminum Alloy 5254-H32
standard
ANSI
heat treatment
Wrought

About 5xxx aluminum alloys

5xxx aluminum alloys are alloyed with magnesium. They are not heat-treatable and gain strength through cold work. They have the best corrosion resistance of the wrought aluminums in marine environments. 5052 covers general sheet work; 5083 and 5086 are common in shipbuilding and pressure vessels.

What else is in Engineering Database

Related comparisons

View each material