Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/Aluminum Alloy 319.0 vs Aluminum Alloy 328.0

Aluminum Alloy 319.0 vs Aluminum Alloy 328.0

Property comparison of Aluminum Alloy 319.0 and Aluminum Alloy 328.0, both aluminum alloy.

Aluminum Alloy12 compared properties
PropertyAluminum Alloy 319.0Aluminum Alloy 328.0Difference
Yield strength90 MPa145 MPa+61%
Tensile strength159 MPa234 MPa+47%
Elongation1.5 %1 %-33%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness55 HB65 HB+18%
Thermal conductivity155 W/m·K155 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000021 1/K0.000021 1/K0%
Melting point516 °C521 °C+1%

Difference is Aluminum Alloy 328.0 relative to Aluminum Alloy 319.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 319.0
standard
ANSI
heat treatment
Cast (F)
Aluminum Alloy 328.0
standard
ANSI
heat treatment
Cast (T6)