Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/Aluminum Alloy 3004-H36 vs Aluminum Alloy 3004-O

Aluminum Alloy 3004-H36 vs Aluminum Alloy 3004-O

Property comparison of Aluminum Alloy 3004-H36 and Aluminum Alloy 3004-O, both aluminum alloy.

Aluminum Alloy12 compared properties
PropertyAluminum Alloy 3004-H36Aluminum Alloy 3004-ODifference
Yield strength228 MPa69 MPa-70%
Tensile strength262 MPa179 MPa-32%
Elongation5 %20 %+300%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness70 HB45 HB-36%
Thermal conductivity159 W/m·K159 W/m·K0%
Specific heat893 J/kg·K893 J/kg·K0%
Coefficient of thermal expansion0.000023 1/K0.000023 1/K0%
Melting point629 °C629 °C0%

Difference is Aluminum Alloy 3004-O relative to Aluminum Alloy 3004-H36. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 3004-H36
standard
ANSI
heat treatment
Wrought
Aluminum Alloy 3004-O
standard
ANSI
heat treatment
Wrought

About 3xxx aluminum alloys

3xxx aluminum alloys carry manganese as the main alloying element. They are not heat-treatable and offer moderate strength with good formability and corrosion resistance. 3003 is the most common general-purpose sheet; 3004 is used for beverage can bodies.