Aluminum Alloy12 compared properties
PropertyAluminum Alloy 2117-T4Aluminum Alloy 2218-T72Difference
Yield strength165 MPa255 MPa+55%
Tensile strength296 MPa331 MPa+12%
Elongation27 %11 %-59%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness70 HB95 HB+36%
Thermal conductivity151 W/m·K151 W/m·K0%
Specific heat875 J/kg·K864 J/kg·K-1%
Coefficient of thermal expansion0.000023 1/K0.000023 1/K0%
Melting point510 °C510 °C0%

Difference is Aluminum Alloy 2218-T72 relative to Aluminum Alloy 2117-T4. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 2117-T4
standard
ANSI
heat treatment
Wrought
Aluminum Alloy 2218-T72
standard
ANSI
heat treatment
Wrought

About 2xxx aluminum alloys

2xxx aluminum alloys are alloyed with copper. They reach the highest strengths in the wrought aluminum family but corrode faster than 5xxx or 6xxx and are difficult to weld. 2024 is the aerospace standard for skin and structure; 2014 is used for forgings.

What else is in Engineering Database

Related comparisons

View each material