Aluminum Alloy11 compared properties
PropertyAluminum Alloy 204.0Aluminum Alloy 242.0Difference
Yield strength193 MPa90 MPa-53%
Tensile strength310 MPa165 MPa-47%
Elongation6 %1 %-83%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Thermal conductivity155 W/m·K155 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000021 1/K0.000021 1/K0%
Melting point532 °C527 °C-1%

Difference is Aluminum Alloy 242.0 relative to Aluminum Alloy 204.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 204.0
standard
ANSI
heat treatment
Cast (T4)
Aluminum Alloy 242.0
standard
ANSI
heat treatment
Cast (T77)