Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/Aluminum Alloy 201.0 vs Aluminum Alloy 242.0

Aluminum Alloy 201.0 vs Aluminum Alloy 242.0

Property comparison of Aluminum Alloy 201.0 and Aluminum Alloy 242.0, both aluminum alloy.

Aluminum Alloy11 compared properties
PropertyAluminum Alloy 201.0Aluminum Alloy 242.0Difference
Yield strength345 MPa138 MPa-60%
Tensile strength414 MPa221 MPa-47%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness110 HB90 HB-18%
Thermal conductivity155 W/m·K155 W/m·K0%
Specific heat880 J/kg·K900 J/kg·K+2%
Coefficient of thermal expansion0.000021 1/K0.000021 1/K0%
Melting point571 °C527 °C-8%

Difference is Aluminum Alloy 242.0 relative to Aluminum Alloy 201.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Aluminum Alloy 201.0
standard
ANSI
heat treatment
Cast (T7)
Aluminum Alloy 242.0
standard
ANSI
heat treatment
Cast (T61)

What else is in Engineering Database

Related comparisons

View each material