Stainless Steel7 compared properties
PropertyAL 29-4C Superferritic Stainless SteelATI 433 Ferritic Stainless SteelDifference
Yield strength552 MPa322 MPa-42%
Tensile strength655 MPa437 MPa-33%
Elongation20 %31 %+55%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,670 kg/m³7,750 kg/m³+1%
Thermal conductivity17 W/m·K20.9 W/m·K+23%
Coefficient of thermal expansion0.000009 1/K0.00001 1/K+12%

Difference is ATI 433 Ferritic Stainless Steel relative to AL 29-4C Superferritic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

AL 29-4C Superferritic Stainless Steel
grade
UNS S44735
standard
ASTM A268/A240
heat treatment
Annealed
ATI 433 Ferritic Stainless Steel
grade
UNS S43300
standard
ASTM A240
heat treatment
Annealed

About ferritic stainless steels

Ferritic stainless steels are magnetic, body-centered cubic, and cannot be hardened by heat treatment. They are cheaper than austenitic grades because they carry little or no nickel. 409 and 439 are the standard automotive exhaust grades; 444 and the superferritic grades (29-4C, E-Brite) handle chloride and seawater service better than 316 at lower nickel cost.