Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Polymer/ABS (high impact) vs BMI Bismaleimide Resin (neat cast Matrimid 5292 type)

ABS (high impact) vs BMI Bismaleimide Resin (neat cast Matrimid 5292 type)

Property comparison of ABS (high impact) and BMI Bismaleimide Resin (neat cast Matrimid 5292 type), both polymer.

Polymer7 compared properties
PropertyABS (high impact)BMI Bismaleimide Resin (neat cast Matrimid 5292 type)Difference
Tensile strength38 MPa50 MPa+32%
Elongation40 %2 %-95%
Poisson ratio0.380.36-5%
Density1,040 kg/m³1,200 kg/m³+15%
Thermal conductivity0.17 W/m·K0.2 W/m·K+18%
Specific heat1,400 J/kg·K1,300 J/kg·K-7%
Coefficient of thermal expansion0.000095 1/K0.000035 1/K-63%

Difference is BMI Bismaleimide Resin (neat cast Matrimid 5292 type) relative to ABS (high impact). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ABS (high impact)
standard
ASTM
BMI Bismaleimide Resin (neat cast Matrimid 5292 type)
standard
ASTM

What else is in Engineering Database