Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free

7175 vs 7475

Property comparison of 7175 and 7475, both aluminum alloy.

Aluminum Alloy7 compared properties
Property71757475Difference
Yield strength455.07 MPa475.76 MPa+5%
Tensile strength524.02 MPa530.92 MPa+1%
Elongation7 %10 %+43%
Elastic modulus70,329 MPa71,019 MPa+1%
Shear modulus26,891 MPa26,201 MPa-3%
Poisson ratio0.330.330%
Density2,796 kg/m³2,796 kg/m³0%

Difference is 7475 relative to 7175. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

7175
grade
7175
standard
MIL-HDBK-5J
heat treatment
Wrought
7475
grade
7475
standard
MIL-HDBK-5J
heat treatment
Wrought

About 7xxx aluminum alloys

7xxx aluminum alloys are alloyed with zinc and reach the highest strengths in the wrought family. Weldability is poor and corrosion resistance trails 5xxx and 6xxx. 7075 is the aerospace standard for highly loaded structure; 7050 trades a small amount of strength for better fracture toughness.