7049 vs 7075

Property comparison of 7049 and 7075, both aluminum alloy.

Aluminum Alloy12 compared properties
Property70497075Difference
Yield strength448 MPa103 MPa-77%
Tensile strength517 MPa228 MPa-56%
Elongation12 %17 %+42%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness135 HB60 HB-56%
Thermal conductivity130 W/m·K130 W/m·K0%
Specific heat860 J/kg·K860 J/kg·K0%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point477 °C477 °C0%

Difference is 7075 relative to 7049. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

7049
standard
ANSI
heat treatment
Wrought
7075
standard
ANSI
heat treatment
Wrought

About 7xxx aluminum alloys

7xxx aluminum alloys are alloyed with zinc and reach the highest strengths in the wrought family. Weldability is poor and corrosion resistance trails 5xxx and 6xxx. 7075 is the aerospace standard for highly loaded structure; 7050 trades a small amount of strength for better fracture toughness.