5CR Mo V vs 9NI 4CO 0.30C
Property comparison of 5CR Mo V and 9NI 4CO 0.30C, both carbon steel.
| Property | 5CR Mo V | 9NI 4CO 0.30C | Difference |
|---|---|---|---|
| Yield strength | 1,482 MPa | 1,310 MPa | -12% |
| Tensile strength | 1,793 MPa | 1,517 MPa | -15% |
| Elongation | 8 % | 10 % | +25% |
| Elastic modulus | 206,843 MPa | 196,501 MPa | -5% |
| Density | 7,778 kg/m³ | 7,750 kg/m³ | 0% |
| Specific heat | 464 J/kg·K | 460 J/kg·K | -1% |
| Reduction in area | 30 % | 40 % | +33% |
Difference is 9NI 4CO 0.30C relative to 5CR Mo V. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
5CR Mo V
- grade
- 5Cr-Mo-V
- standard
- MIL-HDBK-5J
- heat treatment
- Quenched and tempered
9NI 4CO 0.30C
- grade
- 9Ni-4Co-0.30C
- standard
- MIL-HDBK-5J
- heat treatment
- Quenched and tempered
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators