Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/304H Austenitic Stainless Steel (UNS S30409) vs Alloy 904L Super-Austenitic

304H Austenitic Stainless Steel (UNS S30409) vs Alloy 904L Super-Austenitic

Property comparison of 304H Austenitic Stainless Steel (UNS S30409) and Alloy 904L Super-Austenitic, both stainless steel.

Stainless Steel5 compared properties
Property304H Austenitic Stainless Steel (UNS S30409)Alloy 904L Super-AusteniticDifference
Yield strength206.8 MPa220 MPa+6%
Tensile strength517.1 MPa490 MPa-5%
Elongation40 %36 %-10%
Elastic modulus199,955 MPa190,000 MPa-5%
Coefficient of thermal expansion0.000017 1/K0.000015 1/K-8%

Difference is Alloy 904L Super-Austenitic relative to 304H Austenitic Stainless Steel (UNS S30409). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

304H Austenitic Stainless Steel (UNS S30409)
grade
304H
standard
ASTM A240
heat treatment
Annealed
Alloy 904L Super-Austenitic
grade
N08904
standard
ASTM A240/B625
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material