15 5PH vs ATI 15-7 PH (Semi-Austenitic)

Property comparison of 15 5PH and ATI 15-7 PH (Semi-Austenitic), both stainless steel.

Stainless Steel6 compared properties
Property15 5PHATI 15-7 PH (Semi-Austenitic)Difference
Yield strength1,000 MPa380 MPa-62%
Tensile strength1,069 MPa860 MPa-20%
Elongation12 %30 %+150%
Elastic modulus196,000 MPa195,000 MPa-1%
Density7,780 kg/m³7,800 kg/m³0%
Coefficient of thermal expansion0.000011 1/K0.000014 1/K+31%

Difference is ATI 15-7 PH (Semi-Austenitic) relative to 15 5PH. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

15 5PH
grade
S15500
standard
AMS 5659 / AMS 5862
heat treatment
H1025
ATI 15-7 PH (Semi-Austenitic)
grade
UNS S15700
standard
AMS 5520
heat treatment
Condition A (Solution Annealed)

About precipitation-hardening stainless steels

PH grades reach high strength through aging at intermediate temperatures while keeping the corrosion resistance of austenitic or martensitic grades. 17-4 PH and 15-5 PH are the common bar and forging stocks for aerospace and pump shafts. Mechanical properties depend strongly on the aging condition (H900, H1025, H1150).